Composite Material For High Stiffness Parts
A high stiffness plastic boasting excellent printing accuracy and high humidity resistance.
Material Performance
Impact
Strength
13-17 J/m
Heat Deflection
Temperature
65-66°C @ 66 PSI
65°C @ 264 PSI
Flexural
Strength
124-154 MPa
Tensile
Strength
66-68 MPa
Material Highlights
Features
- Excellent stiffness
- High temperature and humidity resistance
- High production speed
- Precise accuracy
Uses
- Assembly jigs and fixtures
- Wind-tunnel testing
- Electrical and mechanical components
Performance Scale
Material Colours
Technical Specifications
Post-Cured Material | Test Method | Metric | U.S. |
Tensile Strength (MPa/PSI) |
ASTM D638 | 66-68 | 6900-9800 |
Tensile Modulus (MPa/KSI) |
ASTM D638 | 7600-11700 | 1100-1700 |
Elongation at Break (%) | ASTM D638 | 1.4-2.4 | 1.4-2.4 |
Flexural Strength (MPa/PSI) |
ASTM D790 | 124-154 | 1800-2230 |
Flexural Modulus (MPa/KSI) |
ASTM D790 | 8300-9800 | 1200-1417 |
Impact Strength (J/m /Ft-lbs/in) |
ASTM D256 | 13-17 | 0.24-0.32 |
Heat Deflection Temperature |
ASTM D 648 @ 66 PSI @ 264 PSI |
65-66 °C 65 °C |
149-151 °F 149 °F |
Glass Transition (Tg) | DMA, E” | 51 °C | 124 °F |
Coefficient of Thermal Expansion (CTE) |
ASTM E 831-93 T Tg (110-150°C): 81-98 |
33-44 81-98 |
18.3-24.2 45-54.4 |
Hardness, Shore D | 92 | 92 |
Liquid Material | Test Method | Value |
Viscosity | @ 30 °C (86 °F) | 1200-1800cps |
Penetration Depth (Dp) | 4.1 mils | |
Critical Exposure (Ec) | 6.9 mJ/cm2 | |
Colour | Blue | |
Solid Density | @ 25 °C (77 °F) | 1.78 g/cm3 |
Liquid Density | @ 25 °C (77 °F) | 1.70 g/cm3 |